MUSCOVITE MICA MINE SCRAP
Properties | Muscovite |
Chemical Formula | KalAlSiO(OH) |
Colour | Ruby and Pale green |
Specific gravity | 2.7 – 3.0 |
Hardness Mohs | 2.8 -3.2 |
Specific heat | 0.206-0.209 |
Thermal Coductivity Cal/ Sec C | 16 x10 |
Coeffiecient of Expansion per C | (9-36) x10 |
Tensile Strength kgf/mm | 30-45 |
Compression Strength kgf/mm | 50-70 |
Modulus of Elasticity kgf/mm | (14-21)x10 |
Calcining Temperature C | 600-800 |
Ignition Loss ( 900 C x3Hrs ) % | 4-5 |
Acid Reaction H SO | Not affected |
Alkali Reaction NaOH | Not affected |
Dielectric Strength Kv/0.1mm | 18-25 |
Dielectric Constant ( 1MHZ) | 6-9 |
Power Factor (50Hz) % | 0.01-0.03 |
Power Factor (1MHz) % | 0.08-0.09 |
Resistivity | 10-10 |
...